4043
Aluminum
Alloy |
Aluminum alloy containing 5% silicon recommended for use on 3003, 3004, 5052 and 6061 grades of aluminum.
Not recommended if deposit is to be subsequently anodized. |
Pre and post heat according to base metal chemistry. |
5356
Aluminum
Alloy |
Aluminum alloy containing 5% manganese recommended for use on 505, 5052, 5083, 5356, 5454 and 5456 aluminum alloys.
Recommended if deposit is to be subsequently anodized. |
Pre and post heat according to base metal chemistry. |